Berlac® Reflexion - test results.

Cross-cut adhesion:Gt0
Scratch resistance 4N and finger nails:no breaking of coating film

Abrasion resistance, 
Crockmeter 2000 double strokes:

no change

Heat storage, 216 hours (90 days) at
90°C:

Gt0, scratch resistance OK no change

Condensed water-constant climate, 
240 hr/40°C at 96% humidity + 1hr regeneration:

Gt0, no change

Hydrolysis test 168 hr/90°C at 96%
humidity (climate chamber):

Gt0, minimal change in appearance

Resistance under the influence of
temperature 24 hr/60°C (Coca Cola,
orange juice, Nivea Sun SPF15,
Nivea cream, sun lotion test blend):

Gt0, no change

Resistance to hand cream and sun
lotion, 24 hr/80°C:

Gt0, scratch resistance OK no change

Steam jet test, 150mm distance, water 
temperature 60°C, 60 sec., pressure 90 bar:

value 0 (in accordance with DIN 55662)

Stone impact test:OK

News

Agenda 2021

Trade Fairs

Due to the current situation with Covid-19, Berlac will not participate in trade fairs in 2021. We would be pleased to present our wide range of products and services to you again in 2022 on various platforms.

Agenda 2022

Berlac exhibiting at PaintExpo

26 - 29 April 2022 | World's leading trade fair for industrial painting technology | Karlsruhe, Germany

Jobs and carreers

Job vacancies

Unfortunately, we have no positions vacant at the moment.

Footer